Check this out!
I found a little first surface mirror that was in "ok" condition for an experiment.
I cut a piece of Aluminum to an angle of less than 45 degrees and used J-B Weld Epoxy to glue the mirror to the Aluminum.
It took over night for it to fully harden.
Then I carefully worked the back of the mirror into a flat piece of wet sand paper facing up on a piece of thick plate glass.
The technique is called lapping. It comes from lapidary, the art of cutting and polishing stones.
I started with 180 grit and went through 320, 400, 600, 1000, & 1500. I had some 2000, but I don't have a fresh sheet.
As you can see, glass wet sands very nicely!
Now I guess I can either try this one or make another one!